Advantages:
20-40%
reduced heeating and Air-conditioner cost - Energy saving
Jointless treatment
Excellent corrosion resistance
Versatile Affinity to any substrate and shapes
Easy and spedy application
No maintenance and easy to patch up in case of any mechanical damage
Protective
embrances are essential over the sprayed on foam and recommeded treatments
are:
Acrylic polymer cementious membrane
Polyurethane elastomeric coatings
Conventional IPS, Tiles, Roofing granules, Coal tar etc.
| PROPERTIES |
C-I
/ 40 |
C-II
/ 50 |
C-III
/ 60 |
| CORE
DENSITY (Kg/m3) |
38
4 |
48
4 |
56
4 |
| COMPRESSIVE
STRENGTH (Kg/cm2) |
2.2
0.2 |
2.7
0.2 |
3.4
0.2 |
| CLOSED
CELL CONTENT (%) |
ABOVE
92 |
ABOVE
92 |
ABOVE
94 |
| THERMAL
CONDUCTIVITY (W/moC) |
| a.
INITIAL |
0.017 |
0.017 |
0.017 |
| b.
AFTER AGEING |
0.022 |
0.022 |
0.022 |
| DIMENSIONAL
STABILITY (%) (lINEAR CHANGE) |
| a.
AT 15oC |
<1 |
<1 |
<1 |
| a.
AT 70oC, 97% RH |
<3 |
<3 |
<3 |
| WATER
VAPOUR PERMEABILITY (g/m2h) |
4.75
0.5 |
4.6
0.4 |
4.75
0.5 |
| FLAME
RETERDENCY * |
4.75
0.5 |
4.6
0.4 |
4.75
0.5 |
| *ONLY
IN THE FIRE RETARDANT GRADE MATERIAL. |
Disclaimer:
This information, given
in good faith, is based on results gained from experience and tests.
However all recommendations or suggestions are made without guarantee,
since the conditions of use are beyond our controls.
We
are pioneers in-situ foaming company and are well conversent with
adapting to all site conditions. Our team of commited engineers and
workmen know only to deliver quality and timely service, for all our
projects.
|